Material Notes:
Isocor™ HW29TL is an ultra low viscosity PA-610 with excellent melt flow characteristics. Isocor™ HW29TL is specifically formulated for thin wall or high speed injection molding applications. This resin is suitable for applications requiring low moisture absorption and greater dimensional stability. This resin can be processed using conventional techniques. Used for thin-wall injection molding, electrical connectors, small parts-high outputInformation provided by Shakespeare Company.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ASTM D 792
Linear Mold Shrinkage 0.011 cm/cm

@Thickness 3.17 mm
0.011 in/in

@Thickness 0.125 in
Mechanical Properties Metric English Comments
Tensile Strength at Break 60.0 MPa
8700 psi
ASTM D 638
Elongation at Break 100 %
100 %
ASTM D 638
Flexural Modulus 2.00 GPa
290 ksi
ASTM D 790
Izod Impact, Notched 0.481 J/cm
0.900 ft-lb/in
ASTM D 256
Taber Abrasion, mg/1000 Cycles 6.0
6.0
ASTM D 1044
Thermal Properties Metric English Comments
Melting Point 215 °C
419 °F
DSC
Deflection Temperature at 0.46 MPa (66 psi) 175 °C
347 °F
ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 66.0 °C
151 °F
ASTM D 648