Shakespeare WP-89 diameter 0.2 mm Warp Polyester Monofilament

Category Polymer , Thermoplastic , Polyester, TP
Manufacturer Shakespeare Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shakespeare WP-89 diameter 0.2 mm Warp Polyester Monofilament.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Paper Machine Clothing MonofilamentHigh molecular weightPolyesterVery high modulusWarp yarn Information provided by Shakespeare Company.
Mechanical Properties Metric English Comments
Elongation at Break 13 %
13 %
Elongation at Yield 3.0 %
3.0 %
at 3 g/D
Thermal Properties Metric English Comments
Shrinkage 10.5 %

@Temperature 200 °C
10.5 %

@Temperature 392 °F