Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shamrock Technologies Fluoro T® 807 Thermoplastic Grade PTFE Additive

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Shamrock Technologies
Trade Name Fluoro T®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shamrock Technologies Fluoro T® 807 Thermoplastic Grade PTFE Additive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction (0.04) and is therefore useful as an internal lubricant processing aid. Because the PTFE particles are inert, processing and the other physical properties of the thermoplastic resin are not adversely affected. The optimum loading is typically 5 to 20 wt% PTFE. As a result of the improved surface wear and slip, thermoplastic products containing FLUORO-T® PTFE, look good longer while in use. The molecular weight and particle size distribution of the Shamrock series of FLUORO-T PTFE powders for thermoplastics are tailored to yield optimum improvements to wear resistance and surface friction, and flow easily during blending.Low FrictionLubricantWear ResistanceInformation provided by Shamrock TechnologiesThe addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction (0.04) and is therefore useful as an internal lubricant processing aid. Because the PTFE particles are inert, processing and the other physical properties of the thermoplastic resin are not adversely affected. The optimum loading is typically 5 to 20 wt% PTFE. As a result of the improved surface wear and slip, thermoplastic products containing FLUORO-T® PTFE, look good longer while in use. The molecular weight and particle size distribution of the Shamrock series of FLUORO-T PTFE powders for thermoplastics are tailored to yield optimum improvements to wear resistance and surface friction, and flow easily during blending.Low FrictionLubricantWear ResistanceInformation provided by Shamrock Technologies.
Physical Properties Metric English Comments
Specific Gravity 2.15 g/cc
2.15 g/cc
Internal method
Bulk Density 0.350 - 0.550 g/cc
0.0126 - 0.0199 lb/in³
ASTM D-4894
Additive Loading 5.0 - 25 %
5.0 - 25 %
When used as an additive
Particle Size 12 µm
12 µm
Mean Value, Laser diffraction; QSOP-5&75
30 µm
30 µm
95%, Laser diffraction; QSOP-5&75
Mechanical Properties Metric English Comments
Coefficient of Friction 0.040
0.040
Thermal Properties Metric English Comments
Melting Point 320 - 330 °C
608 - 626 °F
ASTM-D-4591
Descriptive Properties Value Comments
Appearance Fine powder
Color White
FDA Regulatory Information 21CFR;175.105;175.300;176.170;176.180