Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shandong Dongyue Shenzhou New Material Co DS602 Perfluorinated Ethylene-Propylene Copolymer

Category Polymer , Thermoplastic , Fluoropolymer , FEP
Manufacturer Shandong Dongyue Shenzhou New Material Co
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shandong Dongyue Shenzhou New Material Co DS602 Perfluorinated Ethylene-Propylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Conformable with: Q/DYS 003-2007Fluorinated Ethylene Propylene resin is the copolymer of the TFE and HFP, with good thermal stability, outstanding chemical inertness, good electrical insulation, and low coefficient of friction, enabling thermoplastic processing methods.Main Applications:The low melting resin and heat stress cracking resistant moulding plastic, used for stress cracking resistant requiring and low or medium speed of processing, mainly for heat shrinkable tubes, pumps, valves, piping and lining, wire insulation layer.Information Provided by Shandong Dongyue Shenzhou New Material Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 2.15 - 2.17 g/cc
2.15 - 2.17 g/cc
Volatiles <= 0.10 %
<= 0.10 %
Melt Flow 0.80 - 2.0 g/10 min
0.80 - 2.0 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 27.0 MPa
>= 3920 psi
Elongation at Break >= 320 %
>= 320 %
Thermal Properties Metric English Comments
Melting Point 255 - 275 °C
491 - 527 °F
Electrical Properties Metric English Comments
Dielectric Constant <= 2.15

@Frequency 1.00e+6 Hz
<= 2.15

@Frequency 1.00e+6 Hz
Dissipation Factor <= 0.00070

@Frequency 1.00e+6 Hz
<= 0.00070

@Frequency 1.00e+6 Hz
Descriptive Properties Value Comments
Appearance Translucent particles, without impurities such as metal debris and sand, containing visible black particles percentage point less than 2%
Heat Stress Cracking (%) Crackless