Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shandong Dongyue Shenzhou New Material Co Fluorocarbon Solvent

Category Other Engineering Material
Manufacturer Shandong Dongyue Shenzhou New Material Co
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shandong Dongyue Shenzhou New Material Co Fluorocarbon Solvent.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Conformable with: Q/DYS 012-2007Fluorocarbon solvent is a mixture of perfluorocarbon circular ether. It is a colorless transparent liquid, odorless, nontoxic and uninflammable. It is unsoluble in water, but soluble in organic solvent such as alcohol, ether and acetone. It can carry oxygen efficiently and has excellent electrical property such as high resistance and low power, and widely being used in chemical, electrical and medical industry.Main Applications:It is used as cooling medium of various electrical equipment and insulated fluid, isolation liquid, lubricant, depurative and chemical reaction medium.Information Provided by Shandong Dongyue Shenzhou New Material Co., Ltd.
Physical Properties Metric English Comments
Density 1.73 - 1.78 g/cc

@Temperature 22.0 - 24.0 °C
0.0625 - 0.0643 lb/in³

@Temperature 71.6 - 75.2 °F
pH 6.0 - 7.0
6.0 - 7.0
Thermal Properties Metric English Comments
Boiling Point 80.0 - 120 °C
176 - 248 °F
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Processing Properties Metric English Comments
Moisture Content <= 100 %
<= 100 %
ppm
Descriptive Properties Value Comments
Appearance Colorless transparent liquid
Distillate Content (%) >95
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved