Shin-Etsu Silicones KE-200 Silicone, Potting/Encapsulation RTV

Category Polymer , Thermoset , Silicone , Silicone, RTV, Encapsulation Grade
Manufacturer Shin-Etsu Silicones
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shin-Etsu Silicones KE-200 Silicone, Potting/Encapsulation RTV.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.01 g/cc
1.01 g/cc
Viscosity 2800 cP
2800 cP
Mechanical Properties Metric English Comments
Hardness, Shore A 25
25
Tensile Strength 0.400 MPa
58.0 psi
Thermal Properties Metric English Comments
Thermal Conductivity 0.210 W/m-K
1.46 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Dielectric Strength 20.0 kV/mm
508 kV/in
Dissipation Factor 0.0030

@Frequency 50.0 Hz
0.0030

@Frequency 50.0 Hz
Processing Properties Metric English Comments
Cure Time 4320 min

@Temperature 23.0 °C
72.0 hour

@Temperature 73.4 °F
Descriptive Properties Value Comments
Colors Translucent/Blue
Mix Ratio By Weight 10:01