Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shin-Etsu Silicones KE-5006BU Low Temperature Silicone Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Shin-Etsu Silicones
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shin-Etsu Silicones KE-5006BU Low Temperature Silicone Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ShinEtsu KE5006B U is a phenyl (PVMQ) silicone compound. This product is designed for good low temperature characteristics.Product Features: A broad range of service temperatures from 100 to +260°C (148 to +500°F.)Typical Applications: Low temperature gaskets.Low temperature packing.Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 54
54
Tensile Strength at Break 10.8 MPa
1560 psi
Elongation at Break 570 %
570 %
Tear Strength 31.6 kN/m
180 pli
Die B
Compression Set 28 %

@Temperature 150 °C,
Time 79200 sec
28 %

@Temperature 302 °F,
Time 22.0 hour
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -100 °C
-148 °F
Processing Properties Metric English Comments
Cure Time 240 min

@Temperature 150 °C
4.00 hour

@Temperature 302 °F
Post
Descriptive Properties Value Comments
Cure Agent DCBP
Cure Type Post Cure