Shin-Etsu Silicones KE-581U Silicone Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Shin-Etsu Silicones
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shin-Etsu Silicones KE-581U Silicone Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
KE581U is one of a series of easy processing, general purpose grade silicone rubber bases. It can be used in a variety of applications requiring finishing by molding or extruding with extending filler.Product Features: This product can be blended with KE541U, KE551U, KE561U, and KE571U for intermediate hardnesses. The choice between these bases will depend on specific requirementsTypical Applications: Roll covers.Diaphragms.O-rings and gaskets.Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
DCBP Cure
1.24 g/cc
1.24 g/cc
DBPH Cure
Mechanical Properties Metric English Comments
Hardness, Shore A 78
78
DCBP Cure
78
78
DBPH Cure
Tensile Strength at Break 10.31 MPa
1495 psi
DBPH Cure
11.20 MPa
1625 psi
DCBP Cure
Elongation at Break 350 %
350 %
DCBP Cure
360 %
360 %
DBPH Cure
Tear Strength 12.1 kN/m
69.0 pli
Die B; DCBP Cure
13.0 kN/m
74.0 pli
Die B; DBPH Cure
Compression Set 23 %

@Temperature 150 °C,
Time 79200 sec
23 %

@Temperature 302 °F,
Time 22.0 hour
DCBP Cure
Descriptive Properties Value Comments
Cure Agent DBPH
DCBP
Cure Type Post Cure
Users viewing this material also viewed the following: