Shin-Etsu Silicones KEP-21 Silicone additive

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Shin-Etsu Silicones
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shin-Etsu Silicones KEP-21 Silicone additive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
KEP21 is an additive which can be used in most of the silicone products to improve linear shrinkage.Product Features: Improve linear shrinkage.Excellent dispersion..Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc