Shin-Etsu Silicones KF-6050 Fluid

Category Fluid , Lubricant , Silicone Base
Manufacturer Shin-Etsu Silicones
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shin-Etsu Silicones KF-6050 Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 0.980 g/cc
0.980 g/cc
Viscosity Measurement 7000
7000
cs
Optical Properties Metric English Comments
Refractive Index 1.406
1.406
Descriptive Properties Value Comments
Active (%) 50
Appearance Liquid
Diluent (%) D5
INCI PEG/PPG-18/18 Dimethicone (and) Cyclopentasiloxane (Tentative)