Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shin-Etsu Silicones KSP-300 Fluid

Category Fluid , Lubricant , Silicone Base
Manufacturer Shin-Etsu Silicones
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shin-Etsu Silicones KSP-300 Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 0.300 g/cc
0.300 g/cc
Apparent
1.11 g/cc
1.11 g/cc
True
Volatiles 0.10 %
0.10 %
Particle Size 5.0 µm
5.0 µm
Mechanical Properties Metric English Comments
Hardness, Shore A 40
40
Rubber
Optical Properties Metric English Comments
Refractive Index 1.52
1.52
Descriptive Properties Value Comments
Glyceryl Trioctanoate 5
INCI Diphenyl Dimethicone/Vinyl Diphenyl Methicone/Silsesquioxane Crosspolymer
Isononyl Isonononoate 6
Iso-parafin 4
Nature of Silicone Rubber Core Dimethyl/Diphenyl
Shape Sphere
Swell (g/5g) 2
6cs
3
D5
Users viewing this material also viewed the following: