Shin-Etsu Silicones LIMSâ„¢ KE1950-20A/B Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Shin-Etsu Silicones
Trade Name LIMS™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shin-Etsu Silicones LIMSâ„¢ KE1950-20A/B Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
KE-1950-20 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy pumping through most injection molding systems.FeaturesRapid cure time at elevated temperatureLong pot life at room temperatureApplicationsO-ringsDiaphragmsCappingRubber rollersConnector packingsOther electrical partsInformation Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Viscosity 150000 cP
150000 cP
A
150000 cP
150000 cP
B
Linear Mold Shrinkage 0.021 cm/cm
0.021 in/in
Mechanical Properties Metric English Comments
Hardness, Shore A 20
20
Tensile Strength 6.40 MPa
928 psi
Elongation at Yield 900 %
900 %
100% Modulus 0.000372 GPa
0.0540 ksi
Tear Strength 25.0 kN/m
143 pli
Compression Set 10 %

@Temperature 200 °C,
Time 14400 sec
10 %

@Temperature 392 °F,
Time 4.00 hour
15 %

@Temperature 150 °C,
Time 3600 sec
15 %

@Temperature 302 °F,
Time 1.00 hour
Processing Properties Metric English Comments
Cure Time 5.00 min

@Temperature 120 °C
0.0833 hour

@Temperature 248 °F
Press Cure
60.0 min

@Temperature 150 °C
1.00 hour

@Temperature 302 °F
Post Cure
Descriptive Properties Value Comments
Appearance Translucent
Cure Rate 32
T10 (302°F, ODR)
80
T90 (302°F, ODR)
Regulatory Testing Class VI, FDA