Shinkong Synthetic Fibers Shinite® C501G40 Nylon 6, 40% Glass Filled

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 40% Glass Fiber Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shinkong Synthetic Fibers Shinite® C501G40 Nylon 6, 40% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information from Shinkong Synthetic Fibers Corp.
Physical Properties Metric English Comments
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D792
Water Absorption 1.0 %
1.0 %
ASTM D570
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 147 MPa
21300 psi
ASTM D638
Elongation at Break 2.3 %
2.3 %
ASTM D638
Flexural Yield Strength 216 MPa
31300 psi
ASTM D790
Flexural Modulus 10.3 GPa
1490 ksi
ASTM D790
Izod Impact, Notched 1.47 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
2.76 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ASTM D648
Flammability, UL94 HB
HB