Shinkong Synthetic Fibers Shinite® D201M20 PBT, 20% Mineral Filled

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Mineral Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shinkong Synthetic Fibers Shinite® D201M20 PBT, 20% Mineral Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information from Shinkong Synthetic Fibers Corp.
Physical Properties Metric English Comments
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D792
Water Absorption 0.15 %
0.15 %
ASTM D570
Linear Mold Shrinkage, Flow 0.011 - 0.013 cm/cm
0.011 - 0.013 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.010 - 0.012 cm/cm
0.010 - 0.012 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 53.9 MPa
7820 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Yield Strength 96.1 MPa
13900 psi
ASTM D790
Flexural Modulus 3.53 GPa
512 ksi
ASTM D790
Izod Impact, Notched 0.343 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
0.643 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 97.0 °C
207 °F
ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Constant 4.0
4.0
ASTM D150
Dielectric Strength 20.0 kV/mm
508 kV/in
ASTM D149