Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shinkong Synthetic Fibers Shinite® P305G20 PP, 20% Glass Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Glass Fiber Filler
Manufacturer Shinkong Synthetic Fibers Corp
Trade Name Shinite®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shinkong Synthetic Fibers Shinite® P305G20 PP, 20% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information from Shinkong Synthetic Fibers Corp.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Water Absorption 0.040 %
0.040 %
ASTM D570
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0080 - 0.012 cm/cm
0.0080 - 0.012 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 73.5 MPa
10700 psi
ASTM D638
Elongation at Break 4.5 %
4.5 %
ASTM D638
Flexural Yield Strength 98.1 MPa
14200 psi
ASTM D790
Flexural Modulus 3.53 GPa
512 ksi
ASTM D790
Izod Impact, Notched 0.981 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
1.84 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 150 °C
302 °F
ASTM D648
Flammability, UL94 HB
HB
Users viewing this material also viewed the following: