Shuman 710H Utility Black ABS

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer Shuman
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shuman 710H Utility Black ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Good impact strength, easy processability, good chemical resistanceInformation provided by Shuman Plastics, Inc.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Melt Flow 2.0 - 6.0 g/10 min
2.0 - 6.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 102
102
ASTM D785
Izod Impact, Notched 2.40 - 2.94 J/cm

@Thickness 3.17 mm
4.50 - 5.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 76.1 °C
169 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 177 - 216 °C
350 - 420 °F
Extrusion
204 - 227 °C
400 - 440 °F
Injection
Drying Temperature 76.7 - 93.3 °C

@Time 14400 - 86400 sec
170 - 200 °F

@Time 4.00 - 24.0 hour
Tray Dryer
87.8 - 93.3 °C

@Time 7200 - 86400 sec
190 - 200 °F

@Time 2.00 - 24.0 hour
Dehumidifying Dryer