Sibur ABS 0809 Molding Grade ABS Plastic

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer Sibur
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sibur ABS 0809 Molding Grade ABS Plastic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
With high thermal stability and rigidity for small automobile products and working under higher temperatures.
Physical Properties Metric English Comments
Water Absorption <= 0.30 %
<= 0.30 %
Melt Index of Compound 2.5 - 5.5 g/10 min
2.5 - 5.5 g/10 min
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) >= 8.80 kJ/m²
>= 4.19 ft-lb/in²
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 106 °C
223 °F
Deflection temperature in bending , load unknown
Vicat Softening Point <= 106 °C
<= 223 °F
Chemical Properties Metric English Comments
Styrene Content <= 0.050 %
<= 0.050 %
Descriptive Properties Value Comments
Acrylonitrile Content <.001
Impact Tension Strength >8.8 MPa