Sibur H250 GP Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Sibur
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sibur H250 GP Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polypropylene homopolymer with narrow molecular weight distribution. It features high fluidity, an optimal stabilization package and balanced physical and mechanical properties.general purpose product, used in injection molding applications and composite materials.
Physical Properties Metric English Comments
Melt Flow 25 g/10 min

@Load 2.16 kg,
Temperature 230 °C
25 g/10 min

@Load 4.76 lb,
Temperature 446 °F
GOST 11645
Mechanical Properties Metric English Comments
Tensile Strength, Yield 30.0 MPa
4350 psi
50 mm/min; GOST 11262
Elongation at Yield 11 %
11 %
50 mm/min; GOST 11262
Flexural Modulus 1.40 GPa
203 ksi
5 mm/min; GOST 9550
Izod Impact, Notched (ISO) 2.00 kJ/m²
0.952 ft-lb/in²
GOST 19109
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C
176 °F
GOST 12021
Vicat Softening Point 156 °C

@Load 1.02 kg
313 °F

@Load 2.25 lb
GOST 15088
Descriptive Properties Value Comments
Process Injection Molding
Region Europe/Turkey
Bamberger Polymers Distribution