Sibur PVC S-6558-U-LP Suspension Polyvinyl Chloride (PVC)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Sibur
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sibur PVC S-6558-U-LP Suspension Polyvinyl Chloride (PVC).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
For production of plasticized and rigid articles of general purpose.
Physical Properties Metric English Comments
Density 0.450 - 0.550 g/cc
0.0163 - 0.0199 lb/in³
Collected Volatile Condensable Material <= 0.30 %
<= 0.30 %
Moisture and volatile matters
Thermal Properties Metric English Comments
Decomposition Temperature >= 160 °C
>= 320 °F
Thermal stability, for 5 minutes
Descriptive Properties Value Comments
K-Value 65-67
Mass Share of Vinyl Chloride, mln-1 >10