Material Notes:
Film gradeInformation provided by Sichuan Deyang Chemical Co., LTD
Physical Properties Metric English Comments
Water Absorption <= 0.30 %
<= 0.30 %
GB/T 2914-2008
Molecular Weight >= 50000 g/mol
>= 50000 g/mol
Melt Flow 150 g/10 min
150 g/10 min
GB/T 3682-2000
Ash <= 0.30 %
<= 0.30 %
GB/T 9345.1-2008
Mechanical Properties Metric English Comments
Tensile Strength >= 75.0 MPa
>= 10900 psi
GB/T 1040.2-2006
Elongation at Break >= 2.6 %
>= 2.6 %
GB/T 1040.2-2006
Flexural Strength >= 110 MPa
>= 16000 psi
GB/T 9341-2008
Flexural Modulus >= 3.00 GPa
>= 435 ksi
GB/T 9341-2008
Izod Impact, Unnotched (ISO) >= 3.00 kJ/m²
>= 1.43 ft-lb/in²
GB/T 1843-2008
Thermal Properties Metric English Comments
Melting Point 280 °C
536 °F
GB/T 16582-2008
Flammability, UL94 V-0
V-0