Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Sika Industry SikaTack UltraFast Fast Cure One Part Polyurethane Adhesive

Category Polymer , Adhesive , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Adhesive
Manufacturer Sika Industry
Trade Name SikaTack
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sika Industry SikaTack UltraFast Fast Cure One Part Polyurethane Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Sika UltraFast SikaTack Fast Cure One Part Polyurethane AdhesiveThis revolutionary product uses heat instead of moisture to "pre-cure" the adhesive. The product is heated before applications using a SikaTack oven for extremely fast installation of glass to metal or metal to metal. 1 mm Cut-Off, Excellent non-sag, available in black. Cure Type: Heat and Moisture
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0416 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore A 60 - 70
60 - 70
Tensile Strength, Ultimate 5.52 - 6.21 MPa
800 - 900 psi
Elongation at Break 500 - 600 %
500 - 600 %
Adhesive Bond Strength 4.14 - 4.83 MPa
600 - 700 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.3 °C
200 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Processing Properties Metric English Comments
Cure Time 10.0 - 15.0 min
0.167 - 0.250 hour
Tack-free
1440 min
24.0 hour
Value given per 3/16 inches
Shelf Life 9.00 Month
9.00 Month
Users viewing this material also viewed the following: