Material Notes:
EternaBrite® Premier 251 is a fine, very bright, leafing aluminum pigment with excellent opacity and distinctness of image (D.O.I) for solvent based general industrial coatings. This grade is not recommended for use with chromatic pigments, as the leafing effect will mask the colorant.Applications: General Industrial; Trade & Maintenance
Physical Properties Metric English Comments
Specific Gravity 1.65 g/cc
1.65 g/cc
Bulk Factor 0.073
0.073
Volatiles 26 %
26 %
Particle Size 17 µm
17 µm
Particle Mesh Size <= 325 Mesh
<= 325 Mesh
0.1% retained
Descriptive Properties Value Comments
% Leaf (min) 70
Solvents Mineral Spirits