Sinotek Materials Rigid Graphite Felt Board Heat Insulation Material

Category Carbon , Graphite
Manufacturer Sinotek Materials
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sinotek Materials Rigid Graphite Felt Board Heat Insulation Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Sinotek
Physical Properties Metric English Comments
Bulk Density 0.250 - 0.300 g/cc
0.00903 - 0.0108 lb/in³
Thickness 20000 - 200000 microns
787 - 7870 mil
With Foil or C/C
Thermal Properties Metric English Comments
Thermal Conductivity 0.150 W/m-K

@Temperature 1600 °C
1.04 BTU-in/hr-ft²-°F

@Temperature 2910 °F
Maximum Service Temperature, Air 300 °C
572 °F
Atmosphere
Maximum Service Temperature, Inert 2000 °C
3630 °F
Vacuum
2400 °C
4350 °F
Component Elements Properties Metric English Comments
Carbon, C 98 %
98 %