Material Notes:
Made by suspension polymerization. APPLICATIONS Filler polymer for plastisols. CHARACTERISTICS SolVin 266SC is a suspension resin with very low porosity, small particle size and a very low amount of coarse grains. Used up to 50 phr in formulations for plastisols, it lowers viscosity and considerably reduces ageing of the paste during storage.Information provided by SolVin.
Physical Properties Metric English Comments
Volatile Organic Compounds (VOC) Content <= 0.30 g/l
<= 0.30 g/l
ISO 1269
Apparent Bulk Density 0.700 g/cc
0.0253 lb/in³
Apparent packing density; ISO 1068
Particle Size 30 µm
30 µm
average; ISO 1624
63 µm
63 µm
<0.5 g/kg greater than value; ISO 1624
90 µm
90 µm
<0.05 g/kg greater than value; ISO 1624