Solvay ALKAMULS® A 9 Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name ALKAMULS®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay ALKAMULS® A 9 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Identification: ETHOXYLATED OLEIC ACIDCAS: 9004 – 96 – 0Available in: Asia Pacific, Europe, Latin America and North America Solubility: Dispersible in water. Soluble in most polar and aromatic solvents.Applications: Nonionic emulsifier for metal working formulations. Used in the formulation of water based lubricants, often combined with an anionic.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
pH 5.0 - 7.5
5.0 - 7.5
5% in water; RPG02
Thermal Properties Metric English Comments
Pour Point <= 0.000 °C
<= 32.0 °F
Flash Point >= 100 °C
>= 212 °F
Processing Properties Metric English Comments
Moisture Content <= 1.0 %
<= 1.0 %
RPG16
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Amber liquid
Composition Active content
1
HLB number 11.8
Ionic Charge Nonionic
Saponification number 75-88 mg KOH/g
RPG05