Material Notes:
Description: Good emulsification characteristics, particularly in combination with high or low HLB surfactants to form W/O or O/W emulsions.Chemical Name: ETHOXYLATED SORBITAN TRIOLEATECAS: 9005-70-3; 7732-18-5 Solubility: Water- Dispersible; Mineral Oil-Dispersible; Aromatic- Dispersible; Aliphatic- DispersibleAvailable in: Asia Pacific, Europe, Latin America and North AmericaApplications: ALKAMULS® PSTO-20 is used in the following applications: emulsifier and co-emulsifier for petroleum oils, fats and waxes, lubricant in textile and leather processing, emulsifier for textile finishes and fiberglass lubricant and emulsifier/lubricant in metal working formulations.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
Thermal Properties Metric English Comments
Flash Point >= 149 °C
>= 300 °F
COC; ASTM D92
Optical Properties Metric English Comments
Gardner Color Number <= 9.0
<= 9.0
RP-0138
Chemical Properties Metric English Comments
Total Acid Number <= 2.0
<= 2.0
[mg KOH/g]; RP-0007
Processing Properties Metric English Comments
Moisture Content 4.8 - 5.2 %
4.8 - 5.2 %
Karl Fisher; RP-0327
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Clear Liquid
RP-0064
Composition Active
1
HLB number 11
Hydroxyl Number 39-52 mg KOH/g
RP-0245
Ionic Charge Nonionic
Saponification number 80-95 mg KOH/g
RP-0496