Solvay ANTAROX® BL 225 Surfactant

Category Fluid
Manufacturer Solvay
Trade Name ANTAROX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay ANTAROX® BL 225 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Biodegradable linear alcohol EO/PO. Low foaming non-ionic with excellent hard surface detergency combined to wetting properties. Soluble in water and most organic solvents except paraffinics. Stable in acidic and alkaline solutions. Can be used as a rinse aid forcommercial diswashing or mischellaneous industrial applications. Compliant with the EU's detergent biodegradability regulation.Chemical Name: ETHOXYLATED PROPOXYLATED C8-C10 ALCOHOLSCAS: 68603-25-8; 7732-18-5Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: ANTAROX© BL-225 is a non-ionic surfactant with excellent hard surface detergency combined with wetting properties at low foam levels (up to 50ºC). ANTAROX© BL-225 is stable to acids and soluble in water and most organic solvents except paraffinics. ANTAROX© BL-225 may be used as a rinse aid for commercial dishwashing (detergency), textiles (wetting detergency), and in metal treatment applications.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 0.990 g/cc
0.0358 lb/in³
Viscosity 40 cP
40 cP
Thermal Properties Metric English Comments
Boiling Point 200 °C
392 °F
Flash Point 190 °C
374 °F
Cleveland Open Cup
Optical Properties Metric English Comments
Gardner Color Number <= 3.0
<= 3.0
RP-0138
Processing Properties Metric English Comments
Moisture Content <= 0.50 %
<= 0.50 %
Karl Fisher; RP-0327
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Clear to slightly hazy liquid
RP-0064
Cloud Point 25-29°C
1% Solution, RP-0124
Ionic Charge Nonionic
Neutralization Number <0.5 mg KOH/mg
pH 7, RP-0343