Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Chemicals CASO® Granular Anhydrous Calcium Chloride

Category Ceramic , Halide
Manufacturer Solvay Chemicals
Trade Name CASO®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Chemicals CASO® Granular Anhydrous Calcium Chloride.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CASO® Calcium Chloride technical grade can be used in various applications in industrial, public and private sectors.REACH Registration Number: 01-2119494219-28/ CAS number: 10043-52-4/ EINECS - N°: 233-140-8/ CE - N°: 017-013-00-2 Applications: Civil engineering, dust control, winter road and industrial and domestic dryingInformation provided by Solvay
Physical Properties Metric English Comments
Density <= 0.700 g/cc

@Temperature 0.850 °C
<= 0.0253 lb/in³

@Temperature 33.5 °F
Molecular Weight 111 g/mol
111 g/mol
Descriptive Properties Value Comments
Appearance White or light colored granules
Composition >900 g/kg
CaCl2, Specifications
1.2 g/kg
SO4
27 mg/kg
Fe
30 g/kg
NaCl
947 g/kg
CaCl2
Granulometry 0.07
<1.25 mm
0.5
<2.0 mm
0.83
<2.8 mm
0.99
<5.0 mm
Copyright © lookpolymers.com All Rights Reserved