Solvay Chemicals Soda Solvay® Dense Soda Ash

Category Fluid
Manufacturer Solvay Chemicals
Trade Name Soda Solvay®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Chemicals Soda Solvay® Dense Soda Ash.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Soda Ash Dense is the grade preferred for glass manufacture because its granular properties make it dust-free and reduce the risks of segregation during transport and handling.Applications: Glass industry – Raw Material for melting; Chemical industry – Production of sodium derivatives; Detergents- Alkaline support; Metallurgical processes – Desulfurization of pig iron – Raw material for melting and Flue gas treatment – Removal of acidic components CAS Number: 497-19-8/EINECS: 207-838-8Information provided by Solvay
Physical Properties Metric English Comments
Density 0.890 - 1.09 g/cc
0.0322 - 0.0394 lb/in³
Free flowing, Specification
1.00 g/cc
0.0361 lb/in³
Free flowing, Typical
2.533 g/cc
0.09151 lb/in³
Solubility in Water 21.4 %
21.4 %
pH 11.26
11.26
1% in water
Molecular Weight 106 g/mol
106 g/mol
Thermal Properties Metric English Comments
Melting Point 851 °C
1560 °F
Descriptive Properties Value Comments
Composition <0.02%
Na2SO4, Specification
<0.1%
NaCl, Specification
<110 ppm
CaO, Specification
<130 ppm
MgO, Specification
<30 ppm
Fe2O3, Specification
>99.2%
Na2CO3, Specification
0.0001
Na2SO4, Typical
0.03
NaCl, Typical
0.58
Na2O, Specification
0.584
Na2O, Typical
0.998
Na2CO3, Typical
3 ppm
Fe2O3, Typical
50 ppm
CaO, Typical
65 ppm
MgO, Typical
Granulometry <3%
<0.075 mm, Specification
<5%
>0.6 mm, Specification
>85%
>0.15 mm, Specification
0.01
<0.075 mm, Typical
0.02
>0.6 mm, Typical
0.93
>0.15 mm, Typical