Material Notes:
Identification: ALKYL AMINE NEUTRALIZED ORGANIC PHOSPHATECAS: 68187-67-7Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: DURAPHOS© 178 is a concentrated amine neutralized acid phosphate, providing rust inhibition when blended as a indirect food additive, for lubricating greases calling for incidental food contact complying with 21 CFR 178.3570.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 0.940 - 0.960 g/cc
0.0340 - 0.0347 lb/in³
RPC-11002
Viscosity 1200 cP

@Temperature 40.0 °C
1200 cP

@Temperature 104 °F
Optical Properties Metric English Comments
Gardner Color Number <= 5.0
<= 5.0
RPC-11007
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Viscous liquid
Color Straw