Solvay DURAPHOS® TLP Tri lauryl phosphite

Category Fluid
Manufacturer Solvay
Trade Name DURAPHOS®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay DURAPHOS® TLP Tri lauryl phosphite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chemical Name: TRIALKYL PHOSPHITECAS: 68610-62-8; 108-95-2 Available in: Asia Pacific, Europe, Latin America and North AmericaWater Solubility: Practically Insoluble Applications: DURAPHOS® TLP is a trialkyl phosphite (TLP). It can be used as a lubricant additive and is also an effective stabilizer when used in conjunction with mixed metal heat stabilizers in PVC compounding. Typical use levels range from 0.1 to 2.00%.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 0.872 - 0.882 g/cc
0.0315 - 0.0319 lb/in³
RPC-11002
Viscosity 20 cP
20 cP
Molecular Weight 586 g/mol
586 g/mol
Optical Properties Metric English Comments
Refractive Index 1.454 - 1.459
1.454 - 1.459
RPC-11003
Chemical Properties Metric English Comments
Total Acid Number <= 0.10
<= 0.10
[mg KOH/g]; RPC-11017
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Color <50
APHA, RPC-11002
Composition Alcohol
<5.0%, RP-8075
Phosphorus
0.053
Water
<200 ppm, RPC-11006