Solvay Engineered Polymers DEXFLEX® 810HS TPO  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO) , Polyolefin
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Engineered Polymers DEXFLEX® 810HS TPO  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: DEXFLEX® 810HS is a thermoplastic olefinic elastomer (TPO) that offers excellent weatherability, paintability and processability. This material is designed to exceed the requirements of US 5-mph bumper-impact regulations. Applications: Bumper fascias Information provided by Solvay Engineered Polymers. LyondellBasell acquired Solvay Engineered Polymers in 2008. This grade is not part of the current LyondellBasell product line.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ISO 1183
Linear Mold Shrinkage 0.012 - 0.015 cm/cm
0.012 - 0.015 in/in
as molded; ISO 294
0.015 - 0.018 cm/cm
0.015 - 0.018 in/in
after bake; ISO 294
Melt Flow 14 g/10 min
14 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.0 MPa
2760 psi
150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2
Flexural Modulus 0.800 GPa
116 ksi
80x10x4 mm specimen, 2 mm/min; ISO 178
Impact Test 21.0 J
15.5 ft-lb
multiaxial, 2.2 m/s; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear 100 µm/m-°C

@Temperature -30.0 - 80.0 °C
55.6 µin/in-°F

@Temperature -22.0 - 176 °F
ASTM E228