Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Engineered Polymers DEXFLEX® 826HS TPO  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO) , Polyolefin
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Engineered Polymers DEXFLEX® 826HS TPO  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: DEXFLEX® 826HS is a thermoplastic olefinic elastomer (TPO) designed for automotive exterior applications that require a combination of stiffness, low-temperature impact resistance, and excellent paintability. Applications: Bumper fascias, end caps, air dams, wheel flares, and other large components that must exhibit durable paintability in exterior body colors. Information provided by Solvay Engineered Polymers.LyondellBasell acquired Solvay Engineered Polymers in 2008. This grade is not part of the current LyondellBasell product line.
Physical Properties Metric English Comments
Specific Gravity 0.890 g/cc
0.890 g/cc
ISO 1183
Linear Mold Shrinkage 0.012 - 0.015 cm/cm
0.012 - 0.015 in/in
as molded; ISO 294
0.015 - 0.018 cm/cm
0.015 - 0.018 in/in
after bake; ISO 294
Melt Flow 12 g/10 min
12 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 17.0 MPa
2470 psi
150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2
Flexural Modulus 0.710 GPa
103 ksi
80x10x4 mm specimen, 2 mm/min; ISO 178
Impact Test 18.0 J
13.3 ft-lb
multiaxial, 2.2 m/s; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear 95.0 µm/m-°C

@Temperature -30.0 - 80.0 °C
52.8 µin/in-°F

@Temperature -22.0 - 176 °F
ASTM E228