Material Notes:
Description: DEXFLEX® 900 is a thermoplastic olefinic elastomer (TPO) designed for large automotive exterior applications that require ductile impact properties at low temperatures, excellent paintability, and processability. Applications: Bumper fascias, claddings Information provided by Solvay Engineered PolymersLyondellBasell acquired Solvay Engineered Polymers in 2008. This grade is not part of the current LyondellBasell product line.
Physical Properties Metric English Comments
Specific Gravity 0.980 g/cc
0.980 g/cc
ISO 1183
Linear Mold Shrinkage 0.0082 cm/cm
0.0082 in/in
Melt Flow 21 g/10 min
21 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.8 MPa
2870 psi
ASTM D638M
Flexural Modulus 1.60 GPa
232 ksi
80x10x4 mm specimen, 2 mm/min; ISO 178
Thermal Properties Metric English Comments
CTE, linear 78.0 µm/m-°C

@Temperature -30.0 - 80.0 °C
43.3 µin/in-°F

@Temperature -22.0 - 176 °F
ASTM E228