Material Notes:
Description: DEXFLEX® 990 is a thermoplastic olefinic elastomer (TPO) designed for automotive exterior applications that require a combination of stiffness, low-temperature impact, and excellent processability. Applications: Bumper fascias, and other large components that must exhibit durable paintability or excellent weatherability Information provided by Solvay Engineered PolymersLyondellBasell acquired Solvay Engineered Polymers in 2008. This grade is not part of the current LyondellBasell product line.
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ISO 1183
Linear Mold Shrinkage 0.0090 - 0.011 cm/cm
0.0090 - 0.011 in/in
after bake; ISO 294
Melt Flow 15 g/10 min
15 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 15.3 MPa
2220 psi
150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2
Flexural Modulus 1.14 GPa
165 ksi
80x10x4 mm specimen, 2 mm/min; ISO 178
Impact Test >= 35.0 J
>= 25.8 ft-lb
multiaxial, 2.2 m/s; ASTM D3763