Solvay Engineered Polymers DEXFLEX® E160 TPO  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO) , Polyolefin
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Engineered Polymers DEXFLEX® E160 TPO  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: DEXFLEX® E160 thermoplastic olefinic elastomer (TPO) is designed for extrusion applications that require thermal stability, excellent low-temperature properties, and good dimensional stability over a broad temperature range. This material can be supplied with or without UV stabilizers. Applications: Extrusion and thermoforming or automotive parts, such as luggage racks. Information provided by Solvay Engineered Polymers.LyondellBasell acquired Solvay Engineered Polymers in 2008. This grade is not part of the current LyondellBasell product line.
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D792
Melt Flow 0.58 g/10 min
0.58 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 56
56
ASTM D2240
Tensile Strength, Yield 19.0 MPa
2760 psi
IV, 2 in/min; ASTM D638
Elongation at Break 350 %
350 %
ASTM D638
Flexural Modulus 0.552 GPa
80.1 ksi
Procedure A; ASTM D790
Gardner Impact >= 36.2 J

@Temperature -30.0 °C
>= 26.7 ft-lb

@Temperature -22.0 °F
ASTM D5420-96
>= 36.2 J

@Temperature 23.0 °C
>= 26.7 ft-lb

@Temperature 73.4 °F
ASTM D5420-96