Solvay Engineered Polymers SEQUEL® 1783 Engineered Polyolefin  (discontinued **)

Category Polymer , Thermoplastic , Polyolefin
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Engineered Polymers SEQUEL® 1783 Engineered Polyolefin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: SEQUEL® 1783 engineered polyolefin is designed for large, mold-in-color automotive exterior applications that require dimensional stability over a broad temperature range. This material exhibits excellent high- or low-gloss surface appearance, and processability. SEQUEL® 1783 offers improved scratch and mar resistance compared to typical TPO products. Applications: Exterior cowl grilles, leaf screens, scuff plates, and painted exterior panels. Information provided by Solvay Engineered Polymers.LyondellBasell acquired Solvay Engineered Polymers in 2008. This grade is not part of the current LyondellBasell product line.
Physical Properties Metric English Comments
Specific Gravity 1.09 g/cc
1.09 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm
0.0050 - 0.0080 in/in
as molded; ISO 294
Melt Flow 14 g/10 min
14 g/10 min
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.0 MPa
3050 psi
50 mm/min; ASTM D638
Flexural Modulus 2.00 GPa
290 ksi
I.B., TAN, 0.5 in/min; ASTM D790
Thermal Properties Metric English Comments
CTE, linear 55.0 µm/m-°C

@Temperature -30.0 - 80.0 °C
30.6 µin/in-°F

@Temperature -22.0 - 176 °F
ASTM E228