Solvay Engineered Polymers SEQUEL® 1880 Engineered Polyolefin  (discontinued **)

Category Polymer , Thermoplastic , Polyolefin
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Engineered Polymers SEQUEL® 1880 Engineered Polyolefin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: SEQUEL® 1880 engineered polyolefin is designed for large automotive applications that require dimensional stability over a broad temperature range. This material exhibits excellent processability. Applications: Exterior cargo box covers Information provided by Solvay Engineered Polymers.LyondellBasell acquired Solvay Engineered Polymers in 2008. This grade is not part of the current LyondellBasell product line.
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ISO 1183
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm
0.0050 - 0.0080 in/in
as molded; ISO 294
0.0060 - 0.0090 cm/cm
0.0060 - 0.0090 in/in
after bake; ISO 294
Melt Flow 11 g/10 min
11 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 18.0 MPa
2610 psi
150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2
Flexural Modulus 2.00 GPa
290 ksi
80x10x4 mm specimen, 2 mm/min; ISO 178
Impact Test 19.0 J
14.0 ft-lb
multiaxial, 2.2 m/s; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear 45.0 µm/m-°C

@Temperature -30.0 - 80.0 °C
25.0 µin/in-°F

@Temperature -22.0 - 176 °F
ASTM E228