Solvay GEROPON® TC 42 Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name GEROPON®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay GEROPON® TC 42 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: A paste form of Sodium Methyl Cocoyl Taurate that exhibits good lathering properties. Displays excellent dispersibilty properties in hard water and high electrolyte loads. Compliant with the EU's detergent biodegradability regulation.Chemical Name: SODIUM N-COCONUT ACID-N-METHYL-TAURATECAS: 61791-42-2 Solubility: Soluble in water.Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: GEROPON® TC-42 is a coconut fatty acid derived anionic surfactant with excellent detergency and wetting properties. A mild surfactant with good foam boosting properties, GEROPON® TC-42 exhibits soap like lathering characteristics even in hard water. GEROPON® TC-42 is primarily used as a secondary foaming agent in skin cleanser and shampoo formulations.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
pH 7.0 - 8.0
7.0 - 8.0
10% Solution; RP-0420
Thermal Properties Metric English Comments
Melting Point 12.0 °C
53.6 °F
Chemical Properties Metric English Comments
Ionic Impurities - Fe (Iron) <= 15 ppm
<= 15 ppm
O-PHENANTHROLINE; RP-0277
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Soft, Smooth White Paste
RP-0064
Composition Active
24-26%, EQ WT. 363, RP-0027
Free Amine
<1.5, As Methyltaurine, RP-0793
Free Fatty Acid
<2.0%, EQ. WT. 218, RP-0007
Sodium Chloride
3-6%, RP-0097
Ionic Charge Anionic
Micro Limits <10 CFU/G (No Pathogens)
APC, COA