Material Notes:
Product Description: Mackam LDP is a specially formulated blend of amphoteric and nonionic surfactants that is ideal for use in hard surface cleaners. Mackam LDP is suggested for systems where sodium chloride would be detrimental to the performance of the final product or would cause corrosion problems. Mackam LDP is stable over a broad pH range and is used both as a detergent and hydrotrope in high electrolyte systems. It helps wetting and solubilization in systems containing phosphate and polyphosphates. Uses: All Purpose Cleansers, Steam Cleaners, White Wall Tire Cleaners, Oven Cleaners and Hard Surface CleanersInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
Solids Content 37 - 39 %

@Temperature 105 °C,
Time 5400 sec
37 - 39 %

@Temperature 221 °F,
Time 1.50 hour
1 gram w/Pad
pH 6.0 - 8.0
6.0 - 8.0
Optical Properties Metric English Comments
Gardner Color Number <= 4.0
<= 4.0
Processing Properties Metric English Comments
Shelf Life 48.0 Month
48.0 Month
Descriptive Properties Value Comments
Appearance Clear Liquid