Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay MACKAM® OAB Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name MACKAM®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay MACKAM® OAB Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Mackam OAB is a 30% active aqueous solution of caprylamidopropyl betaine. It acts as an effective hydrotrope to couple nonionic surfactants into systems containing moderate amounts of electrolyte. Mackam OAB is a low foamer that provides good detergency in systems that require high cloud points. Mackam OAB is not available in the UK and certain other countries. INCI Name: Caprylamidopropyl Betaine CAS: 73772-46-0 EINECS: 277-600-6Infrared Spectrum: Matches StandardFoam: Time-30sec Max and Height-80mL MaxUses: All Purpose Cleaners, Car Washes, Wax Strippers and Acid Bowl CleanersInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
Solids Content 36 - 38 %
36 - 38 %
Moisture Balance
pH 6.5 - 8.0
6.5 - 8.0
Optical Properties Metric English Comments
Gardner Color Number <= 3.0
<= 3.0
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Clear Liquid
Composition Bacteria Counts
<10
Gram Negative Bacteria
Absent
Sodium Chloride
6-7%
Copyright © lookpolymers.com All Rights Reserved