Solvay MACKAZOLINE® C Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name MACKAZOLINE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay MACKAZOLINE® C Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Mackazoline C is a cationic surface-active agent. It is oil soluble, water dispersible, and contains no solvents. Mackazoline C offers good emulsification properties and stability. It can be neutralized with common acids to give amine salts or combined with alkyl halides and dialkyl sulfates to form quaternary ammonium compounds. Mackazoline C can also be used as a reaction intermediate in production of very mild cosmetic ingredients. INCI Name: Coco Hydroxyethyl Imidazoline CAS: 61791-38-6 EINECS: 263-170-7Uses: Corrosion Inhibitors, Emulsifier, Industrial Cleaners & Detergents, Agricultural Aids, Petroleum Recovery and Chemical IntermediateInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
Optical Properties Metric English Comments
Gardner Color Number <= 4.0
<= 4.0
Chemical Properties Metric English Comments
Total Acid Number <= 1.0
<= 1.0
Processing Properties Metric English Comments
Shelf Life 48.0 Month
48.0 Month
Descriptive Properties Value Comments
Appearance Clear to Hazy Liquid
Composition Amine Value
200-240
Imidazoline
80-100%, MW 277
Weight/Gallon 7.76 lbs