Description: An optimum blend of anionic and amphoteric surfactants to provide a base concentrate having excellent foaming properties and low irritancy.Chemical Name: AMPHOTERIC/ANIONIC SURFACTANT BLENDCAS: 68650-39-5, 68585-47-7, 107-41-5EINECS : 272-043-5/205-788-1/203-489-0Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: MIRACARE 2MCA is an optimum blend of anionic and amphoteric surfactants to provide a base concentrate having excellent foaming properties and low irritancy.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
Solids Content >= 46 %
>= 46 %
Karl fisher, Includes Diol; RP-0327
pH 8.0 - 8.5
8.0 - 8.5
20% Solution; RP-0420
Thermal Properties Metric English Comments
Crystallization Temperature <= 0.000 °C
<= 32.0 °F
Processing Properties Metric English Comments
Moisture Content <= 54 %
<= 54 %
Karl Fisher; RP-0327
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Composition Active
>38.2%, %Active=%Solids-%Sodium Chloride-%Sodium Sulfate
Formaldehyde
150-200 ppm, RP-0197
Hexylene Glycol
8.5-9.5%, DIOL, RP-0222
Sodium Chloride
6.5-7.3%, RP-0098
Sodium Sulfate
<0.5%, RP-0555
Ionic Charge Anionic