Solvay RHEOZAN Biopolymer

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Renewable/Recycled Polymer
Manufacturer Solvay
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHEOZAN Biopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Biopolymer: very stable in acid media (such as sulfuric acid). Highly pseudoplastic.Identification: SUCCINOGLYCAN GUMCAS: 73667 – 50 – 2Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: Industrial and household cleaners.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 0.750 - 0.850 g/cc
0.0271 - 0.0307 lb/in³
Particle Size <= 300 µm
<= 300 µm
98% min; TI-2087-2
pH 7.0 - 9.0
7.0 - 9.0
0.2% aq. Sol.; TI-2088
Brookfield Viscosity >= 3250 cP
>= 3250 cP
0.3% in 1% HCl, LV3 rpm spindle n°2 after 24 h at 40°C; TI-2102-1
Descriptive Properties Value Comments
Appearance Creamy, fine powder
Loss on drying <13%
TI-0515-2