Material Notes:
Description: Linear Calcium dodecylbenzene sulfonate, 60% active , useful in emulsifier blends where low viscosity is needed.Identification: MIXTURE OF LINEAR DODECYLBENZENSULPHONIC ACID, CALCIUM SALT AND ISOBUTYL ALCOHOL.CAS: 26264 – 06 – 2 ; 78 – 83 – 1Solubility: Dispersible in water. Soluble in most polar and aromatic solvent.Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: EmulsifierInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 0.980 g/cc
0.0354 lb/in³
pH 5.0 - 7.0
5.0 - 7.0
5% in water; RPG02
Thermal Properties Metric English Comments
Pour Point 0.000 °C
32.0 °F
Flash Point 28.0 °C
82.4 °F
Processing Properties Metric English Comments
Moisture Content <= 1.0 %
<= 1.0 %
RPG16
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Viscous liquid
Composition Active
0.6
HLB number 8.6
Ionic Charge Anionic