Solvay RHODACAL® 70/B Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODACAL® 70/B Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description Anionic, linear Calcium dodecylbenzene sulfonate, 70% active , useful in emulsifier blendsIdentification: MIXTURE OF LINEAR DODECYLBENZENSULPHONIC ACID, CALCIUM SALT AND ISOBUTYL ALCOHOL.CAS: 26264 – 06 – 2 ; 78 – 83 – 1p>Solubility: Dispersible in water. Soluble in most polar and aromatic solvent.Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: EmulsifierInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
pH 5.0 - 7.0
5.0 - 7.0
5% in water; RPG02
Thermal Properties Metric English Comments
Pour Point 0.000 °C
32.0 °F
Flash Point 28.0 °C
82.4 °F
Processing Properties Metric English Comments
Moisture Content <= 1.0 %
<= 1.0 %
RPG16
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Viscous liquid
Composition Active
0.7
HLB number 8.6
Ionic Charge Anionic