Solvay RHODAFAC® RS-610 Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODAFAC® RS-610 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Moderate foaming. Exceptional electrolyte tolerance. Versatile product with wide ranging applications. Used as emulsifier, penetrant, antistat and dry-cleaning detergent. Emulsifies pesticides in liquid fertilizer. Used in caustic boil and peroxide bleaching of cotton. Also used in alkaline detergents and pulp and paper processing. Coupling properties and hard surface detergency.Chemical Name: COMPLEX ORGANIC PHOSPHATE ESTER, FREE ACIDCAS: 9046-01-9Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: RHODAFAC® RS-610 is a very effective APE-Free primary anionic surfactant for acrylic, styrene/acrylic, and vinyl/acrylic latex syntheses. RHODAFAC® RS-610 exhibits desirable properties in films, including corrosion inhibition, heat and light stability and clarity.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Solids Content 100 %
100 %
Chemical Properties Metric English Comments
Total Acid Number 75 - 85
75 - 85
KOH to First INFL. PT.; RP-0427
Processing Properties Metric English Comments
Moisture Content <= 0.80 %
<= 0.80 %
Karl Fisher; RP-0327
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Hazy liquid
RP-0064
Color <200
APHA, RP-0134
Composition Nonionic Content
<10%, RP-0351
Critical Micelle Concentration 2E-05
Ionic Charge Anionic