Solvay RHODAPEX® EST-30/BLB Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODAPEX® EST-30/BLB Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chemical Name: Sodium Trideceth(3) SulfateCAS: 25446-78-0Available in: Asia Pacific, Europe, Latin America and North America Applications: RHODAPEX EST-30/BLB is an APE-Free emulsifier for acrylic, vinyl/acrylic and styrene/acrylic latexes. Also effective emulsifier for making high solid acrylic latex system.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
pH 7.5 - 8.5
7.5 - 8.5
10% Solution; RP-0420
Optical Properties Metric English Comments
Gardner Color Number <= 2.0
<= 2.0
RP-0138
Processing Properties Metric English Comments
Shelf Life 9.00 Month
9.00 Month
Descriptive Properties Value Comments
Appearance Clean, Clear liquid
RP-0064
Cloud Point <14°C
RP-0123
Composition Anionic Active
29-30%, EQ. WT 434, RP-0033
Nonionics
<2%, RP-0966
Sodium Bicarbonate
0.5-0.7%, Rp-0078
Sodium Chloride
<1%, RP-0098
Sodium Sulfate
<1.5%, RP-0555