Material Notes:
Identification: BENZYLTRIPHENYLPHOSPHONIUM CHLORIDECAS: 1100 – 88 – 5Available in: Asia Pacific, Europe, Latin America and North America Applications: Benzyltriphenylphosphonium Chloride (tpp-zc) is a crystalline quaternary phosphonium salt which finds its application in Wittig reactions and in Phase Transfer Catalysis. Literature reports its use as a component in printing inks and as a fluoropolymer cure accelerator.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance White crystalline solid
Assay >97%
AM6502
Purity >97%