Solvay RHODAPON® TL-40/A Surfactant

Category Fluid
Manufacturer Solvay
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODAPON® TL-40/A Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Rhodapon® TL-40/A is formaldehyde preserved clear light liquid with excellent foaming characteristics. It is a milder Lauryl sulfate grade and it has enhanced compatibility with fragrances and electrolytes.Chemical Name: FATTY ALCOHOL SULFATECAS: 117875-77-1Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: RHODAPON TL-40/A is a versatile toiletry raw material which combines optimum performance with excellent foaming characteristics. The viscosity of these derived formulations can be adjusted by the addition of inorganic salts. The mildness of a product formulated with RHODAPON TL-40/A may be improved by the inclusion of cocoamphoacetates. Used in many personal care applications such as shampoos, hair color treatments, liquid soaps, creams and lotions, and related cosmetic productsInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
pH 6.5 - 7.0
6.5 - 7.0
10% Solution; RP-0420
Viscosity 40 - 120 cP
40 - 120 cP
RP-0596
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Clear Light Liquid
RP-0064
Color Yellow
Composition Active
>40%, EQ. WT. 422, RP-0033
Free Amine
<2.0%, EQ. WT. 149, RP-0040
Free Oil
<2.0%, RP-17303
TEA Chloride
0.3-1.0%, EQ. WT. 185.7, RP-0098
Odor Faint, Characteristic